1 COATING SYSTEMS · EXPAND FOR DETAILS
Labels explained
- PLUS
PLUS means additional plasma nitriding before PVD coating (duplex). It supports the PVD coating on through-hardened tool steel. nitriding hardness depth: 0.02–0.05 mm. Depending on the system, PLUS is optional or always included. PLUS is used for stamping, forming and die casting. Through-hardened tool steels with a tempering temperature above 500 °C are required.
- M-Guard optional
- Additional diffusion treatment for plastics applications. Can be combined with the marked PVD coatings.
- F-series available
- Also available as a separate F variant for specific testing and approval requirements. See the coating details for application areas.
ALTINOVAAlTiNAvailable as a Nova serviceFor Asgard systemsHardness in HV: 3300 ± 350Coating thickness in micrometres: 2–4Maximum operating temperature in degrees Celsius: 800
- Composition
- AlTiN
- Hardness
- 3300 ± 350 HV
- Coating thickness
- 2–4 µm
- Max. operating temperature
- 800 °C
- Coating temperature
- 450–480 °C
- Coefficient of friction
- 0.5
- Colour
- Anthracite
- Plus option / duplex
- Not specified
- Finishing as required
- Available
Recommended applications according to the coating overview
- Metal forming
- Machining
Technical guidance based on the NOVA coating overview and Apex datasheets. Properties depend on the system and application. We confirm suitability and current specifications with you.
Open the Nova service portfolio as an image ↗